| US$100.00 | 1 Square Meter (MOQ) |
| Carbon Content: | ≥99% |
| Thermal Conductivity: | 0.08-0.14W/m.k |
| Volume Density: | 0.12-0.14g/cm3 |
| Tensile Strength: | 0.14Mpa |
| Crushing stress at 10% compression: | 8-10N/cm2 |
| Processing Temperature: | 2500ºC |
| Thermal Conductivity: | 0.15-0.25W/m.k |
| Specific Resistance: | 0.17-0.22 |
| Carbon Content: | ≥99% |
| Ash Content: | ≤0.3 |
| Moisture Absorption: | ≤2.0 |
| Processing Temperature: | 1450-2500ºC |